Z3CT12 Stainless Steels to NF A 35-573

Z3CT12 - Specification & Application

  • NF A 35-573 - Stainless steels for general purposes. Plates, wide strips and strips
  • NF A 35-578 - Iron and steel. Stainless steel for high temperature application

Iron and steel. Stainless steel for high temperature application

Chemical composition(wt.%) of Z3CT12 grade: to NF A 35-573

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.030
Si - 0.75
Mn - 0.08
P - 0.040
S - 0.015
Cr 10.50 12.50
Mo - -
Ni - -
N - 0.025
Ti - 0.60

Z3CT12 - Detail

Iron and steel. Stainless steel for high temperature application

Mechanical properties of grade Z3CT12 NF A 35-573

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
291 (≥) 481 (≥) 14 13 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 134

Physical properties of grade Z3CT12 NF A 35-573

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
354 (≥) 118 (≥) 11 22 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 234
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
166 234 628

Equivalent Grade

Equivalent Products

We can customize the production of Z3CT12 grade, contact us for the best solution.