Z50CMNNb21-09-02Az Stainless Steels to NF A 35-579

Z50CMNNb21-09-02Az - Specification & Application

  • NF A 35-579 - Valve steels and alloys for internal combustion engines

Valve steels and alloys for internal combustion engines

Chemical composition(wt.%) of Z50CMNNb21-09-02Az grade: to NF A 35-579

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.45 0.55
Si - 0.45
Mn 8.00 10.00
P - 0.040
S - 0.030
Cr 20.00 22.00
Ni 3.50 5.00
Mo - -
Nb/Ta 1.80 2.50
W 0.80 1.50
No 0.40 0.60

Z50CMNNb21-09-02Az - Detail

Valve steels and alloys for internal combustion engines

Mechanical properties of grade Z50CMNNb21-09-02Az NF A 35-579

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
992 (≥) 576 (≥) 23 33 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 244

Physical properties of grade Z50CMNNb21-09-02Az NF A 35-579

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
879 (≥) 484 (≥) 41 32 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 414
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
832 787 438

Equivalent Products

We can customize the production of Z50CMNNb21-09-02Az grade, contact us for the best solution.