Z53CMN21-09Az Stainless Steels to NF A 35-579

Z53CMN21-09Az - Specification & Application

  • NF A 35-579 - Valve steels and alloys for internal combustion engines

Valve steels and alloys for internal combustion engines

Chemical composition(wt.%) of Z53CMN21-09Az grade: to NF A 35-579

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.48 0.58
Si - 0.25
Mn 8.00 10.00
P - 0.040
S - 0.030
Cr 20.00 22.00
Ni 3.25 4.50
Mo - -
N 0.38 0.50

Z53CMN21-09Az - Detail

Valve steels and alloys for internal combustion engines

Mechanical properties of grade Z53CMN21-09Az NF A 35-579

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
615 (≥) 667 (≥) 11 22 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 322

Physical properties of grade Z53CMN21-09Az NF A 35-579

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
993 (≥) 958 (≥) 31 24 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 422
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
124 161 669

Equivalent Grade

Equivalent Products

We can customize the production of Z53CMN21-09Az grade, contact us for the best solution.