Iron and steel. Stainless steel for high temperature application
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.04 | 0.08 | ||
Si | - | 0.75 | ||
Mn | - | 2.00 | ||
P | - | 0.040 | ||
S | - | 0.015 | ||
Cr | 16.00 | 18.00 | ||
Mo | 12.00 | 14.00 | ||
Ni | 2.00 | 2.50 | ||
B | 0.0015 | 0.0060 |
Iron and steel. Stainless steel for high temperature application
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
742 (≥) | 262 (≥) | 13 | 11 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 211 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
451 (≥) | 581 (≥) | 23 | 31 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 441 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
356 | 122 | 575 |
We can customize the production of Z6CND17-13B grade, contact us for the best solution.
–sales@specificsteel.com