Z6CNNb18-10F Stainless Steels to NF A 36-613

Z6CNNb18-10F - Specification & Application

  • NF A 36-613 - General purpose forgings. Stainless steels

General purpose forgings. Stainless steels

Chemical composition(wt.%) of Z6CNNb18-10F grade: to NF A 36-613

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.060
Si - 0.75
Mn - 2.00
P - 0.040
S - 0.015
Cr 17.00 19.00
Mo - -
Ni 9.00 11.00
N - 0.050
Nb 10×C 1.00

Z6CNNb18-10F - Detail

General purpose forgings. Stainless steels

Mechanical properties of grade Z6CNNb18-10F NF A 36-613

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
565 (≥) 817 (≥) 24 43 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 231

Physical properties of grade Z6CNNb18-10F NF A 36-613

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
219 (≥) 474 (≥) 22 33 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 323
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
396 972 418

Equivalent Products

We can customize the production of Z6CNNb18-10F grade, contact us for the best solution.