Z6CNNb18-12B Stainless Steels to NF A 35-578

Z6CNNb18-12B - Specification & Application

  • NF A 35-578 - Iron and steel. Stainless steel for high temperature application
  • NF A 49-214 - Steel tubes. Seamless austenitic steel tubes for use at high temperatures. Dimensions (with normal tolerances). Technical conditions of delivery

Steel tubes. Seamless austenitic steel tubes for use at high temperatures. Dimensions (with normal tolerances). Technical conditions of delivery

Chemical composition(wt.%) of Z6CNNb18-12B grade: to NF A 35-578

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.08
Si - 0.75
Mn - 2.00
P - 0.040
S - 0.015
Cr 17.00 19.00
Mo 11.00 13.00
Ni - -
B 0.0015 0.0060
Nb 10×C -

Z6CNNb18-12B - Detail

Steel tubes. Seamless austenitic steel tubes for use at high temperatures. Dimensions (with normal tolerances). Technical conditions of delivery

Mechanical properties of grade Z6CNNb18-12B NF A 35-578

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
788 (≥) 472 (≥) 31 43 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 441

Physical properties of grade Z6CNNb18-12B NF A 35-578

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
838 (≥) 522 (≥) 24 13 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 132
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
759 397 696

Equivalent Grade

Equivalent Products

We can customize the production of Z6CNNb18-12B grade, contact us for the best solution.