Iron-Nickel-Cobalt Alloy, Bars and Forgings, 53Fe - 29Ni - 17Co, Low Expansion, Glass Sealing
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.04 | ||
Si | - | 0.20 | ||
Mn | - | 0.50 | ||
Ni | - | 29.00 | ||
Cr | - | 0.20 | ||
Al | - | 0.10 | ||
Cu | - | 0.20 | ||
Ti | - | 0.10 | ||
Fe | - | 53.00 | ||
Mo | - | 0.20 | ||
Co | - | 17.00 | ||
W | - | - | ||
Mg | - | 0.10 | ||
Zr | - | 0.10 |
Iron-Nickel-Cobalt Alloy, Bars and Forgings, 53Fe - 29Ni - 17Co, Low Expansion, Glass Sealing
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
325 (≥) | 288 (≥) | 23 | 43 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 311 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
593 (≥) | 413 (≥) | 22 | 24 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 244 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
116 | 116 | 781 |