N07002 Stainless Steels

N07002 - Specification & Application

Steel for exhaust valves

Chemical composition(wt.%) of N07002 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 -
Si 0.08 -
Mn 2.25 -
P - -
S - -
Cr 16.0 -
Ni - remaining

N07002 - Detail

Steel for exhaust valves

Mechanical properties of grade N07002

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
253 (≥) 466 (≥) 11 42 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 441

Physical properties of grade N07002

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
335 (≥) 282 (≥) 31 42 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 241
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
688 174 522