N1310 Stainless Steels

N1310 - Specification & Application

non-magnetic steel

Chemical composition(wt.%) of N1310 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Si 0.50 1.00
Mn 17.00 21.00
P - 0.035
S - 0.030
Cr 11.00 15.00
Ni 1.00 2.00
Mo 0.30 0.70
N - 0.30

N1310 - Detail

non-magnetic steel

Mechanical properties of grade N1310

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
787 (≥) 244 (≥) 13 21 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 342

Physical properties of grade N1310

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
436 (≥) 468 (≥) 23 14 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 244
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
985 288 661

Equivalent Grade

We can customize the production of N1310 grade, contact us for the best solution.
sales@specificsteel.com