NiCr20TiAl Superalloys to ISO 683-15 (1992)

NiCr20TiAl - Specification & Application

  • ISO 683-15 (1992) - Heat-treatable steels, alloy steels and free-cutting steels -- Part 15: Valve steels for internal combustion engines

Heat-treatable steels, alloy steels and free-cutting steels -- Part 15: Valve steels for internal combustion engines

Chemical composition(wt.%) of NiCr20TiAl grade: to ISO 683-15 (1992)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.10
Si - 1.00
Mn - 1.00
P - 0.020
S - 0.015
Cr 18.00 21.00
Mo - -
Ni 65.00 -
Al 1.00 1.80
Fe - 3.00
Co - 2.00
B - 0.008
Cu - 0.20
Ti 1.80 2.70

NiCr20TiAl - Detail

Heat-treatable steels, alloy steels and free-cutting steels -- Part 15: Valve steels for internal combustion engines

Mechanical properties of grade NiCr20TiAl ISO 683-15 (1992)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
883 (≥) 497 (≥) 31 31 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 221

Physical properties of grade NiCr20TiAl ISO 683-15 (1992)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
418 (≥) 191 (≥) 34 22 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 233
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
935 624 294