NiCr28FeSiCe Stainless Steels to BS EN 10095

NiCr28FeSiCe - Specification & Application

  • BS EN 10095 - Heat resisting steels and nickel alloys

Heat resisting steels and nickel alloys

Chemical composition(wt.%) of NiCr28FeSiCe grade: to BS EN 10095

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.05 0.12
Si 2.50 3.00
Mn - 1.00
P - 0.020
S - 0.015
Cr 26.00 29.00
Ni 45.00 -
Al - -
Fe 21.00 25.00
Cu - 0.30
Ce 0.03 0.09

NiCr28FeSiCe - Detail

Heat resisting steels and nickel alloys

Mechanical properties of grade NiCr28FeSiCe BS EN 10095

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
388 (≥) 136 (≥) 33 33 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 244

Physical properties of grade NiCr28FeSiCe BS EN 10095

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
866 (≥) 629 (≥) 14 22 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 132
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
543 423 494

Equivalent Products