NiFe25Cr20NbTi Stainless Steels to ISO 683-15 (1992)

NiFe25Cr20NbTi - Specification & Application

  • ISO 683-15 (1992) - Heat-treatable steels, alloy steels and free-cutting steels -- Part 15: Valve steels for internal combustion engines

Heat-treatable steels, alloy steels and free-cutting steels -- Part 15: Valve steels for internal combustion engines

Chemical composition(wt.%) of NiFe25Cr20NbTi grade: to ISO 683-15 (1992)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Si - 1.00
Mn - 1.00
P - 0.030
S - 0.015
Cr 18.00 21.00
Mo - -
Ni remaining -
Al 0.30 1.00
Fe 23.00 28.00
Nb+Ta 1.00 2.00
B - 0.008

NiFe25Cr20NbTi - Detail

Heat-treatable steels, alloy steels and free-cutting steels -- Part 15: Valve steels for internal combustion engines

Mechanical properties of grade NiFe25Cr20NbTi ISO 683-15 (1992)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
574 (≥) 456 (≥) 24 43 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 221

Physical properties of grade NiFe25Cr20NbTi ISO 683-15 (1992)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
138 (≥) 457 (≥) 33 42 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 434
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
117 282 199

Equivalent Products

We can customize the production of NiFe25Cr20NbTi grade, contact us for the best solution.
sales@specificsteel.com