Nivco-10 Stainless Steels to SAE J 467 (1968)

Nivco-10 - Specification & Application

  • SAE J 467 (1968) - Special Purpose Alloys ("Superalloys")

Special Purpose Alloys ("Superalloys")

Chemical composition(wt.%) of Nivco-10 grade: to SAE J 467 (1968)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 0.20
Mn - 0.35
Cr - -
Ni - 22.50
Mo - -
Co - remaining
W - -
Al - 0.22
Cu - -
Ti - 1.75
Fe - 0.50
Zr - 0.62

Nivco-10 - Detail

Special Purpose Alloys ("Superalloys")

Mechanical properties of grade Nivco-10 SAE J 467 (1968)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
171 (≥) 197 (≥) 43 14 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 242

Physical properties of grade Nivco-10 SAE J 467 (1968)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
597 (≥) 328 (≥) 14 33 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 314
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
937 814 572

Equivalent Grade

Equivalent Products

We can customize the production of Nivco-10 grade, contact us for the best solution.