C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Cu(%) |
---|---|---|---|---|---|---|---|
0.09~0.15 | ≤0.30 | 0.25~0.55 | ≤0.045 | ≤0.045 | ≤0.30 | ≤0.30 | ≤0.30 |
High plasticity and toughness and welding performance, good pressure processing performance, but low strength.
Load small parts, spacers, rivets, the anchor bolt, colter, funnel, roof, low carbon steel wire, plates, welded pipe, bars, split cotters, and stamping parts, components etc.
GB/T 700-1988 standadr:
Regardless of rank, the chemical composition and mechanical properties (σ s, σ b, the delta and the cold bending) are to be guaranteed
Rolling plate and rod of products, the mechanical properties of the guarantee condition, can according to product characteristics and application requirements, in the standard separately
GB 700-1979 standard
A1 the mechanical properties of the steel guarantee (σ s, σ b, the delta and the cold bending), B1 steel guarantee the chemical composition of the same with Q195
A1 steel cold bending test is additional guarantee conditions
1 no special steel of steel
Proof strength Rp0.2(MPa) |
Tensile strength Rm(MPa) |
Impact energy KV(J) |
Elongation at fracture A(%) |
Reduction in cross section on fracture Z(%) |
As-Heat-Treated Condition | Brinell hardness(HBW) |
---|---|---|---|---|---|---|
553(≥) | 283(≥) | 14 | 23 | 14 | Solution and Aging,Annealing,Ausaging,Q+T,etc | 111 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J/kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
781(≥) | 983(≥) | 13 | 41 | 22 | Solution and Aging,Annealing,Ausaging,Q+T,etc | 414 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0)N/mm2 |
Creep rupture strength (10000h) (Rp1,0)N/mm2 |
|||||
288 | 117 | 497 |
Product type | Products | Dimension | Processes | Deliver Status |
---|---|---|---|---|
Plates/Sheets | Plates/Sheets | 0.08-200mm(T)*W*L | Forging,hot rolling and cold rolling | Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting |
Steel Bar | Round Bar,Flat Bar,Square Bar | Φ8-1200mm*L | Forging,hot rolling and cold rolling,Cast | Black,Rough Turning,Shot Blasting, |
Coil/Strip | Steel Coil/Steel Strip | 0.03-16.0x1200mm | Cold-Rolled&Hot-Rolled | Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting |
Pipes/Tubes | Seamless Pipes/Tubes,Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion,Cold Drawn,Welded | Annealed,Solution and Aging,Q+T,ACID-WASHED |
Steel grade | Dimension | Shape | Unit | Quantity | Delivery state | Query |
---|---|---|---|---|---|---|
SkD-11 Round Bar Stock | Φ30-Φ350 | Round Bar | Kgs | 3102 | Hot-Rolled+Annealed+black | Enquiry |
17-4PH Coil Stock | 0.08*200mm | Coil or Strip | Kgs | 1623 | Cold-Rolled+Annealed | Enquiry |
D2 Round bar | Φ25-Φ380mm | Round Bar | Kgs | 45325 | Hot-Rolled+Annealed+black | Enquiry |
Cr8 flat bar | 12*355*L | Flat or Square bar | Kgs | 3965 | Forged+Annealed+black | Enquiry |
17-4PH Round Bar | Φ5-300mm*L | Round Bar | Kgs | 46958 | Hot-Rolled+Annealed+black | Enquiry |
17-4PH plate | 8-45*1200*3000mm | Plate or Sheet | Tons | 4.9 | Hot-Rolled+Annealed+black | Enquiry |
Cr12MoV | 12-160(T)*310-610(W)*L | Plate or Sheet | Tons | 12.38 | Hot-Rolled+Annealed+black | Enquiry |
1.2601 | 12-160(T)*310-610(W)*L | Plate or Sheet | Tons | 11.22 | Hot-Rolled+Annealed+black | Enquiry |
IncoloyA-286 / GH 2132 Stock | Φ8-65mm*L | Round Bar | Kgs | 489 | Hot-Rolled+Annealed+black | Enquiry |
Incoloy800 round bar | Φ115*1400 | Round Bar | Kgs | 169 | Hot-Rolled+Annealed+black | Enquiry |
17-7PH / 631 Coil & Strip, Sheet Stock | 0.3-3.0*10-180mm | Coil or Strip | Kgs | 1236.22 | Cold-Rolled+Annealed | Enquiry |
X22CrMoV12-1 / 1.4923 | Φ17mm | Round Bar | Kgs | 300 | Hot-Rolled+Annealed+black | Enquiry |
1.2083 Forged Plate | T:105-185mm*W:510*L | Plate or Sheet | Tons | 26 | Forged+QT | Enquiry |
X22CrMoV12-1 / 1.4923 | Φ30mm | Round Bar | Kgs | 300 | Hot-Rolled+Annealed+black | Enquiry |
1.4882 strip/sheet/plate stock | 3.5x200x1000-2000mm | Coil or Strip | Kgs | 200 | Cold-Rolled+Annealed | Enquiry |
A387 F5 & Grade 5 sheet Coil strip | 0.5mmx200mmxC | Coil or Strip | Tons | 3 | Cold-Rolled+Annealed | Enquiry |
A387 F5 & Grade 5 Hot Coil stock | Select | Tons | 3 | Hot-Rolled+Annealed+black | Enquiry | |
T45Cr5Si3 Round Bar | Dia.40mm | Round Bar | Kgs | 500 | Hot-Rolled+Annealed+black | Enquiry |
UNS K30960(VIM+ESR) Bright Round Bar | Dia.22mm | Round Bar | Kgs | 50 | Hot-Rolled+Annealed+black | Enquiry |
SA-437 Grade B4B/SUS 616 /422 Forged Bar | Dia.160xL | Round Bar | Kgs | 2120 | Forged+QT | Enquiry |