S18200 Stainless Steels

S18200 - Specification & Application

Ferritic Chromium Molybdenum Free-Machining Stainless Steel (18-2FM)

Chemical composition(wt.%) of S18200 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Mn - 2.50
Si - 1.00
P - 0.04
S 0.15 -
Cr 17.50 19.50
Ni - -
Mo 1.50 2.50

S18200 - Detail

Ferritic Chromium Molybdenum Free-Machining Stainless Steel (18-2FM)

Mechanical properties of grade S18200

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
999 (≥) 924 (≥) 43 21 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 341

Physical properties of grade S18200

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
339 (≥) 533 (≥) 23 22 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 311
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
173 443 529

Equivalent Products

We can customize the production of S18200 grade, contact us for the best solution.
sales@specificsteel.com