S20400 Stainless Steels

S20400 - Specification & Application

S20400

Chemical composition(wt.%) of S20400 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.030
Si - 1.00
Mn 7.00 9.00
P - 0.04
S - 0.03
Cr 15.0 17.0
Ni 1.50 3.00
N 0.15 0.30

S20400 - Detail

S20400

Mechanical properties of grade S20400

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
117 (≥) 594 (≥) 33 43 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 222

Physical properties of grade S20400

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
927 (≥) 512 (≥) 42 33 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 141
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
143 683 639

Equivalent Grade

Equivalent Products

We can customize the production of S20400 grade, contact us for the best solution.
sales@specificsteel.com