S30403 Special Alloy

Chemical composition%of the ladle analysis of gradeS30403

C(%)Si(%)Mn(%)P(%)S(%)Cr(%)Ni(%)
0.031.02.00.0450.0318.0-20.08.0-12.0
This standard specifies the stainless steel rods order contents, classification, code, size, shape, weight and allowable deviation, technical requirements, test methods, inspection rules, packaging, logo and certificate of quality.This standard applies to the size is not more than 250 mm hot rolled and forged stainless steel rods.The supply and demand both sides talks things over, can also supply the size larger than 250 mm hot rolled and forged stainless steel rods.

Mechanical properties of gradeS30403

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
425(≥) 921(≥) 31 14 31 Solution and Aging,Annealing,Ausaging,Q+T,etc 312

Physical properties of grade S30403

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
441(≥) 747(≥) 33 34 41 Solution and Aging,Annealing,Ausaging,Q+T,etc 232
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
431 891 947

S30403 Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED