Chemical composition(wt.%) of S42200 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.20 0.25
Mn 0.50 1.00
Si - 0.50
P - 0.025
S - 0.025
Cr 11.00 12.50
Ni 0.50 1.00
Mo 0.90 1.25
W 0.90 1.25
V 0.20 0.30

S42200 - Detail

Martensitic Chromium Molybdenum Nickel Wolfram Stainless Steel (422)

Mechanical properties of grade S42200

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
386 (≥) 137 (≥) 42 23 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 112

Physical properties of grade S42200

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
485 (≥) 123 (≥) 11 12 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 243
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
879 636 591