SA-240 S42900 Stainless Steels to SA-240/SA-240M

SA-240 S42900 - Specification & Application

  • SA-240/SA-240M - Specification for Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Specification for Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Chemical composition(wt.%) of SA-240 S42900 grade: to SA-240/SA-240M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Mn - 1.00
Si - 1.00
P - 0.04
S - 0.03
Cr 14.00 16.00
Ni - -
Mo - 0.75

SA-240 S42900 - Detail

Specification for Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Mechanical properties of grade SA-240 S42900 SA-240/SA-240M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
779 (≥) 933 (≥) 44 31 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 133

Physical properties of grade SA-240 S42900 SA-240/SA-240M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
526 (≥) 293 (≥) 32 41 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 423
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
884 147 916

Equivalent Products

We can customize the production of SA-240 S42900 grade, contact us for the best solution.
sales@specificsteel.com