Specification for Ni-Fe-Cr-Mo-Cu Low-Carbon Alloy (UNS N08904), Ni-Fe-Cr-Mo-Cu-N Low-Carbon Alloys (UNS N08925, UNS N08031, and UNS N08926), and Cr-Ni-Fe-N Low-Carbon Alloy (UNS R20033) Bar and Wire
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.12 | ||
Si | - | 0.30 | ||
Mn | - | 0.80 | ||
Cr | - | 19.00 | ||
Ni | - | 14.00 | ||
Mo | - | - | ||
Co | - | - | ||
W | - | - | ||
Al | - | - | ||
Cu | - | - | ||
Ti | - | - | ||
Fe | - | remaining | ||
Nb | - | 1.60 |
Specification for Ni-Fe-Cr-Mo-Cu Low-Carbon Alloy (UNS N08904), Ni-Fe-Cr-Mo-Cu-N Low-Carbon Alloys (UNS N08925, UNS N08031, and UNS N08926), and Cr-Ni-Fe-N Low-Carbon Alloy (UNS R20033) Bar and Wire
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
786 (≥) | 126 (≥) | 14 | 24 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 344 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
459 (≥) | 837 (≥) | 44 | 31 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 241 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
681 | 947 | 987 |
We can customize the production of SB-649 R20033 grade, contact us for the best solution.