STS304LTPY Stainless Steels to D 3588 (2009)

STS304LTPY - Specification & Application

  • D 3588 (2009) - Large diameter welded stainless steel pipes

Large diameter welded stainless steel pipes

Chemical composition(wt.%) of STS304LTPY grade: to D 3588 (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.030
Cr 18.00 20.00
Ni 9.00 13.00
Mo - -
N - -

STS304LTPY - Detail

Large diameter welded stainless steel pipes

Mechanical properties of grade STS304LTPY D 3588 (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
881 (≥) 963 (≥) 12 34 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 343

Physical properties of grade STS304LTPY D 3588 (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
869 (≥) 237 (≥) 11 14 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 123
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
427 687 899