SUH 4 Stainless Steels to G 4311 (2011)

SUH 4 - Specification & Application

  • G 4311 (2011) - Heat-resisting steel bars and wire rods

Heat-resisting steel bars and wire rods

Chemical composition(wt.%) of SUH 4 grade: to G 4311 (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.75 0.85
Si 1.75 2.25
Mn 0.20 0.60
P - 0.03
S - 0.03
Cr 19.00 20.50
Ni 1.15 1.65
Mo - -

SUH 4 - Detail

Heat-resisting steel bars and wire rods

Mechanical properties of grade SUH 4 G 4311 (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
638 (≥) 649 (≥) 33 34 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 321

Physical properties of grade SUH 4 G 4311 (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
858 (≥) 788 (≥) 33 23 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 141
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
715 421 266

Equivalent Products

We can customize the production of SUH 4 grade, contact us for the best solution.
sales@specificsteel.com