T11346 Tool Die Steels

T11346 - Specification & Application

High-Speed Tool Steel

Chemical composition(wt.%) of T11346 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 1.22 1.30
Si 0.40 0.65
Mn 0.20 0.40
P - 0.030
S - 0.030
Cr 3.70 4.20
Mo 8.00 8.50
V 3.00 3.30
W 1.90 2.20
Co 7.80 8.80

T11346 - Detail

High-Speed Tool Steel

Mechanical properties of grade T11346

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
777 (≥) 862 (≥) 14 33 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 133

Physical properties of grade T11346

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
898 (≥) 286 (≥) 41 43 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 412
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
648 142 819

Equivalent Grade

Equivalent Products

We can customize the production of T11346 grade, contact us for the best solution.