Chemical composition(wt.%) of T20819 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.32 0.45
Si 0.20 0.50
Mn 0.20 0.50
P - 0.030
S - 0.030
Cr 4.00 4.75
Mo 0.30 0.55
V 1.75 2.20
W 3.75 4.50
Ni+Cu - 0.75
Co 4.00 4.50

T20819 - Detail

Hot-Work Tool Steel

Mechanical properties of grade T20819

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
686 (≥) 668 (≥) 21 13 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 144

Physical properties of grade T20819

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
398 (≥) 753 (≥) 44 21 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 223
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
242 315 875

Equivalent Grade