T20821 Tool Die Steels

T20821 - Specification & Application

Hot-Work Tool Steel

Chemical composition(wt.%) of T20821 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.26 0.36
Si 0.15 0.50
Mn 0.15 0.40
P - 0.030
S - 0.030
Cr 3.00 3.75
Mo - -
V 0.30 0.60
W 8.50 10.00
Ni+Cu - 0.75

T20821 - Detail

Hot-Work Tool Steel

Mechanical properties of grade T20821

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
466 (≥) 394 (≥) 44 21 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 241

Physical properties of grade T20821

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
436 (≥) 317 (≥) 24 11 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 243
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
276 377 225

Equivalent Grade

Equivalent Products

We can customize the production of T20821 grade, contact us for the best solution.