T41907 Tool Die Steels

T41907 - Specification & Application

Shock-Resisting Tool Steel

Chemical composition(wt.%) of T41907 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.45 0.55
Si 0.20 1.00
Mn 0.20 0.90
P - 0.030
S - 0.030
Cr 3.00 3.50
Mo 1.30 1.80
V - 0.35
W - -
Ni+Cu - 0.75

T41907 - Detail

Shock-Resisting Tool Steel

Mechanical properties of grade T41907

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
958 (≥) 471 (≥) 23 34 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 133

Physical properties of grade T41907

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
362 (≥) 193 (≥) 31 23 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 323
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
725 473 443