T7 Tool Die Steels

T7 - Specification & Application

High-Speed Tool Steel

Chemical composition(wt.%) of T7 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.70 0.75
Si 0.20 0.40
Mn 0.20 0.40
Cr 4.50 5.00
Mo - -
V 1.50 1.80
W 13.50 14.50

T7 - Detail

High-Speed Tool Steel

Mechanical properties of grade T7

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
494 (≥) 931 (≥) 33 13 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 122

Physical properties of grade T7

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
592 (≥) 651 (≥) 32 21 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 232
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
619 788 418

Equivalent Products

We can customize the production of T7 grade, contact us for the best solution.