U11952 Structural Steel to GB/T 700-2006

U11952 - Specification & Application

  • GB/T 700-2006 - Carbon structural steels
  • ISO 630:1995 - 标准内容

Carbon structural steels

Chemical composition(wt.%) of U11952 grade: to GB/T 700-2006

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Si - 0.3
Mn - 0.5
P - 0.035
S - 0.04
Cr - 0.3
Ni - 0.3
Cu - 0.3
N - 0.0080

U11952 - Detail

This standard applies to steel product standards, technical specifications of the finished product chemical composition of the provisions of the allowable deviation.

Mechanical properties of grade U11952 GB/T 700-2006

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
519 (≥) 222 (≥) 12 12 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 444

Physical properties of grade U11952 GB/T 700-2006

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
451 (≥) 446 (≥) 12 42 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 442
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
615 153 626

Equivalent Products

We can customize the production of U11952 grade, contact us for the best solution.
sales@specificsteel.com