W23318 Stainless Steels

W23318 - Specification & Application

Low alloy steel arc welding electrode (14018-M1)

Chemical composition(wt.%) of W23318 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Ni 13.00 15.00
Cr 17.00 19.00
Al - -
Cu - -
Ti - -
Fe - -
N - -
Mo 1.75 2.75
V - -

W23318 - Detail

Low alloy steel arc welding electrode (14018-M1)

Mechanical properties of grade W23318

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
493 (≥) 362 (≥) 21 23 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 114

Physical properties of grade W23318

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
648 (≥) 236 (≥) 42 44 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 224
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
111 432 294

Equivalent Products

We can customize the production of W23318 grade, contact us for the best solution.