X12Cr13E Stainless Steels to ISO 4954

X12Cr13E - Specification & Application

  • ISO 4954 - Steels for cold heading and cold extruding

Steels for cold heading and cold extruding

Chemical composition(wt.%) of X12Cr13E grade: to ISO 4954

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.09 0.15
Si - 1.00
Mn - 1.00
P - 0.040
S - 0.030
Cr 11.50 13.50
Ni - 1.00
Mo - -

X12Cr13E - Detail

Steels for cold heading and cold extruding

Mechanical properties of grade X12Cr13E ISO 4954

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
128 (≥) 534 (≥) 44 13 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 122

Physical properties of grade X12Cr13E ISO 4954

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
347 (≥) 966 (≥) 24 44 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 342
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
241 228 255

Equivalent Grade

Equivalent Products

We can customize the production of X12Cr13E grade, contact us for the best solution.