X2CrNi12 Stainless Steels to ISO 15510 (2010)

X2CrNi12 - Specification & Application

  • ISO 15510 (2010) - Stainless steels -- Chemical composition
  • ISO 16143-1 (2004) - Stainless steels for general purposes -- Part 1: Flat products
  • ISO 9328-7 (2011) - Steel flat products for pressure purposes - Technical delivery conditions - Part 7: Stainless steels
  • ISO/TS 15510 (2003) - Stainless steels - Chemical composition

Stainless steels - Chemical composition

Chemical composition(wt.%) of X2CrNi12 grade: to ISO 15510 (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 1.00
Mn - 1.50
P - 0.040
S - 0.015
Cr 10.50 12.50
Ni 0.30 1.10
Mo - -
N - 0.03

X2CrNi12 - Detail

Stainless steels - Chemical composition

Mechanical properties of grade X2CrNi12 ISO 15510 (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
762 (≥) 738 (≥) 24 32 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 143

Physical properties of grade X2CrNi12 ISO 15510 (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
578 (≥) 476 (≥) 14 41 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 222
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
228 153 973

Equivalent Products

We can customize the production of X2CrNi12 grade, contact us for the best solution.
sales@specificsteel.com