X2CrNiMoN18-12-4 Stainless Steels to NF EN 10028-7

X2CrNiMoN18-12-4 - Specification & Application

  • NF EN 10028-7 - Flat products made of steels for pressure purposes - Part 7: Stainless steels
  • NF EN 10088-1 - Stainless steels - Part 1: List of stainless steels
  • NF EN 10088-2 - Stainless steels - Part 2: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes

Stainless steels - Part 2: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes

Chemical composition(wt.%) of X2CrNiMoN18-12-4 grade: to NF EN 10028-7

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.030
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.015
Cr 16.50 19.50
Mo 3.00 4.00
Ni 10.50 14.00
N 0.10 0.20

X2CrNiMoN18-12-4 - Detail

Stainless steels - Part 2: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes

Mechanical properties of grade X2CrNiMoN18-12-4 NF EN 10028-7

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
755 (≥) 442 (≥) 23 33 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 143

Physical properties of grade X2CrNiMoN18-12-4 NF EN 10028-7

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
664 (≥) 278 (≥) 11 31 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 323
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
536 434 888

Equivalent Products