Chemical composition(wt.%) of X33CrNiMnN23-8 grade: to NF EN 10090

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.28 0.38
Si 0.50 1.50
Mn 1.50 3.50
P - 0.045
S - 0.030
Cr 22.00 24.00
Ni 7.00 9.00
Mo - 0.50
W - 0.50
N 0.25 0.35

X33CrNiMnN23-8 - Detail

Valve steels and alloys for internal combustion engines

Mechanical properties of grade X33CrNiMnN23-8 NF EN 10090

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
341 (≥) 162 (≥) 13 34 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 143

Physical properties of grade X33CrNiMnN23-8 NF EN 10090

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
664 (≥) 349 (≥) 21 34 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 411
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
618 111 797