X39Cr13 Stainless Steels to ISO 15510 (2010)

X39Cr13 - Specification & Application

  • ISO 15510 (2010) - Stainless steels -- Chemical composition
  • ISO 16143-1 (2004) - Stainless steels for general purposes -- Part 1: Flat products
  • ISO 6931-2 - Stainless steels for springs - Part 2: Narrow strip
  • ISO/TS 15510 (2003) - Stainless steels - Chemical composition

Stainless steels - Chemical composition

Chemical composition(wt.%) of X39Cr13 grade: to ISO 15510 (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.36 0.42
Si - 1.00
Mn - 1.50
P - 0.040
S - 0.030
Cr 12.50 14.50
Ni - -
Mo - -
N - -

X39Cr13 - Detail

Stainless steels - Chemical composition

Mechanical properties of grade X39Cr13 ISO 15510 (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
165 (≥) 834 (≥) 44 31 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 321

Physical properties of grade X39Cr13 ISO 15510 (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
739 (≥) 276 (≥) 21 21 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 123
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
886 346 511

Equivalent Products

We can customize the production of X39Cr13 grade, contact us for the best solution.