X3CrNiMo13-4 Stainless Steels to NF EN 10028-7

X3CrNiMo13-4 - Specification & Application

  • NF EN 10028-7 - Flat products made of steels for pressure purposes - Part 7: Stainless steels
  • NF EN 10088-1 - Stainless steels - Part 1: List of stainless steels
  • NF EN 10088-2 - Stainless steels - Part 2: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes
  • NF EN 10088-3 - Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes
  • NF EN 10222-5 - Steel forgings for pressure purposes - Part 5: Martensitic, austenitic and austenitic-ferritic stainless steels
  • NF EN 10250-4 - Open die steel forgings for general engineering purposes - Part 4: Stainless steels
  • NF EN 10272 - Stainless steel bars for pressure purposes

Stainless steel bars for pressure purposes

Chemical composition(wt.%) of X3CrNiMo13-4 grade: to NF EN 10028-7

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Si - 0.70
Mn - 1.50
P - 0.040
S - 0.015
Cr 12.00 14.00
Mo 0.30 0.70
Ni 3.50 4.50
N 0.020 -

X3CrNiMo13-4 - Detail

Stainless steel bars for pressure purposes

Mechanical properties of grade X3CrNiMo13-4 NF EN 10028-7

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
533 (≥) 196 (≥) 33 33 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 412

Physical properties of grade X3CrNiMo13-4 NF EN 10028-7

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
733 (≥) 949 (≥) 32 44 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 213
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
472 141 493

Equivalent Products

We can customize the production of X3CrNiMo13-4 grade, contact us for the best solution.