X53CrMnNiN21-9 Stainless Steels to ISO 683-15 (1992)

X53CrMnNiN21-9 - Specification & Application

  • ISO 683-15 (1992) - Heat-treatable steels, alloy steels and free-cutting steels -- Part 15: Valve steels for internal combustion engines

Heat-treatable steels, alloy steels and free-cutting steels -- Part 15: Valve steels for internal combustion engines

Chemical composition(wt.%) of X53CrMnNiN21-9 grade: to ISO 683-15 (1992)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.48 0.58
Si - 0.25
Mn 8.00 10.00
P - 0.050
S - 0.030
Cr 20.00 22.00
Mo - -
Ni 3.25 4.50
N 0.35 0.50

X53CrMnNiN21-9 - Detail

Heat-treatable steels, alloy steels and free-cutting steels -- Part 15: Valve steels for internal combustion engines

Mechanical properties of grade X53CrMnNiN21-9 ISO 683-15 (1992)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
469 (≥) 134 (≥) 13 13 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 222

Physical properties of grade X53CrMnNiN21-9 ISO 683-15 (1992)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
323 (≥) 412 (≥) 44 34 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 433
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
821 739 291

Equivalent Products

We can customize the production of X53CrMnNiN21-9 grade, contact us for the best solution.
sales@specificsteel.com