X53CrMnNiNbN21-9 Stainless Steels to NF EN 10090

X53CrMnNiNbN21-9 - Specification & Application

  • NF EN 10090 - Valve steels and alloys for internal combustion engines

Valve steels and alloys for internal combustion engines

Chemical composition(wt.%) of X53CrMnNiNbN21-9 grade: to NF EN 10090

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.48 0.58
Si - 0.45
Mn 8.00 10.00
P - 0.045
S - 0.030
Cr 20.00 22.00
Ni 3.25 4.50
Mo - -
N 0.38 0.50
C+N 0.90 -

X53CrMnNiNbN21-9 - Detail

Valve steels and alloys for internal combustion engines

Mechanical properties of grade X53CrMnNiNbN21-9 NF EN 10090

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
151 (≥) 145 (≥) 32 23 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 332

Physical properties of grade X53CrMnNiNbN21-9 NF EN 10090

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
478 (≥) 719 (≥) 14 13 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 432
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
414 611 463

Equivalent Products

We can customize the production of X53CrMnNiNbN21-9 grade, contact us for the best solution.