X6CrNiMo17-12-2 Stainless Steels to ISO 6931-2

X6CrNiMo17-12-2 - Specification & Application

  • ISO 6931-2 - Stainless steels for springs - Part 2: Narrow strip

Stainless steels for springs - Part 2: Narrow strip

Chemical composition(wt.%) of X6CrNiMo17-12-2 grade: to ISO 6931-2

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.07
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.030
Cr 16.50 18.50
Mo 2.00 2.50
Ni 10.50 13.50

X6CrNiMo17-12-2 - Detail

Stainless steels for springs - Part 2: Narrow strip

Mechanical properties of grade X6CrNiMo17-12-2 ISO 6931-2

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
363 (≥) 682 (≥) 33 31 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 211

Physical properties of grade X6CrNiMo17-12-2 ISO 6931-2

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
226 (≥) 391 (≥) 41 32 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 111
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
827 167 494

Equivalent Products

We can customize the production of X6CrNiMo17-12-2 grade, contact us for the best solution.