X6CrNiTi18 10E Stainless Steels to ISO 4954

X6CrNiTi18 10E - Specification & Application

  • ISO 4954 - Steels for cold heading and cold extruding

Steels for cold heading and cold extruding

Chemical composition(wt.%) of X6CrNiTi18 10E grade: to ISO 4954

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.030
Cr 17.00 19.00
Ni 9.00 12.00
Mo - -
Ti 5×C% 0.80

X6CrNiTi18 10E - Detail

Steels for cold heading and cold extruding

Mechanical properties of grade X6CrNiTi18 10E ISO 4954

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
762 (≥) 376 (≥) 13 13 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 244

Physical properties of grade X6CrNiTi18 10E ISO 4954

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
497 (≥) 741 (≥) 24 22 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 443
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
552 999 931

Equivalent Products

We can customize the production of X6CrNiTi18 10E grade, contact us for the best solution.