X8NiCrAlTi32-21 Stainless Steels to ISO 15510 (2010)

X8NiCrAlTi32-21 - Specification & Application

  • ISO 15510 (2010) - Stainless steels -- Chemical composition
  • ISO 16143-3 (2005) - Stainless steels for general purposes -- Part 3: Wire
  • ISO 4955 (2005) - Heat-resistant steels
  • ISO 9328-5 - Steel plates and strips for pressure purposes - Technical delivery conditions - Part 5: Weldable fine grain steels, thermomechanically rolled
  • ISO 9328-7 (2011) - Steel flat products for pressure purposes - Technical delivery conditions - Part 7: Stainless steels

Steel flat products for pressure purposes - Technical delivery conditions - Part 7: Stainless steels

Chemical composition(wt.%) of X8NiCrAlTi32-21 grade: to ISO 15510 (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Si - 1.00
Mn - 1.50
P - 0.015
S - 0.015
Cr 19.00 23.00
Ni 30.00 34.00
Al 0.15 0.60
Ti 0.15 0.60
Cu - 0.70

X8NiCrAlTi32-21 - Detail

Steel flat products for pressure purposes - Technical delivery conditions - Part 7: Stainless steels

Mechanical properties of grade X8NiCrAlTi32-21 ISO 15510 (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
912 (≥) 929 (≥) 11 21 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 211

Physical properties of grade X8NiCrAlTi32-21 ISO 15510 (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
955 (≥) 211 (≥) 41 24 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 314
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
449 152 442

Equivalent Products

We can customize the production of X8NiCrAlTi32-21 grade, contact us for the best solution.