XC38 Air 9160/C Aviation and Aero Steel to AIR 9160 C

XC38 Air 9160/C - Specification & Application

  • AIR 9160 C - wrought steels used in aeronautical constructions

wrought steels used in aeronautical constructions

Chemical composition(wt.%) of XC38 Air 9160/C grade: to AIR 9160 C

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.35 0.40
Si 0.10 0.40
Mn 0.50 0.80
P - 0.035
S - 0.035

XC38 Air 9160/C - Detail

XC38 Air 9160C wrought steels used in aeronautical constructions

Mechanical properties of grade XC38 Air 9160/C AIR 9160 C

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
547 (≥) 954 (≥) 11 12 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 143

Physical properties of grade XC38 Air 9160/C AIR 9160 C

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
552 (≥) 422 (≥) 41 34 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 412
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
655 478 289

Equivalent Grade

Equivalent Products

We can customize the production of XC38 Air 9160/C grade, contact us for the best solution.