XH32T Stainless Steels

XH32T - Specification & Application

Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Chemical composition(wt.%) of XH32T grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Si - 0.70
Mn - 0.70
P - 0.030
S - 0.020
Cr 19.00 22.00
Ni 30.00 34.00
Mo - -
Al - 0.50
Ti 0.25 0.60
Fe - remaining

XH32T - Detail

Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Mechanical properties of grade XH32T

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
313 (≥) 647 (≥) 44 44 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 123

Physical properties of grade XH32T

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
361 (≥) 382 (≥) 22 23 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 134
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
219 185 166