XH51BMTЮ/KΦK-BД Special Alloy

Chemical composition%of the ladle analysis of gradeXH51BMTЮ/KΦK-BД

C(%)Si(%)Mn(%)Cr(%)Ni(%)Mo(%)V(%)W(%)Co(%)B(%)Al(%)Ti(%)
Max 0.08Max 0.035Max 0.039.0-12.0Balance5.00-7.000.20-0.805.00-6.5014.0-15.5Max 0.0023.90-4.802.20-2.90
XH51BMTЮ/KΦK-BД

Mechanical properties of gradeXH51BMTЮ/KΦK-BД

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
185(≥) 164(≥) 21 24 23 Solution and Aging,Annealing,Ausaging,Q+T,etc 422

Physical properties of grade XH51BMTЮ/KΦK-BД

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
856(≥) 547(≥) 33 24 11 Solution and Aging,Annealing,Ausaging,Q+T,etc 214
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
241 888 318

XH51BMTЮ/KΦK-BД Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED