XH58B Stainless Steels

XH58B - Specification & Application

Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Chemical composition(wt.%) of XH58B grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 0.15
Mn - 1.00
P - -
S - -
Cr 39.00 41.00
Ni - remaining
Mo - -
Al - -
Ti - -
Fe - 0.80
W 0.50 1.50

XH58B - Detail

Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Mechanical properties of grade XH58B

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
144 (≥) 661 (≥) 43 23 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 323

Physical properties of grade XH58B

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
686 (≥) 547 (≥) 33 23 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 313
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
717 347 246