XH65MBy Stainless Steels

XH65MBy - Specification & Application

Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Chemical composition(wt.%) of XH65MBy grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.02
Si - 0.10
Mn - 1.00
P - -
S - -
Cr 14.50 16.50
Ni - remaining
Mo 15.00 17.00
Al - -
Ti - -
Fe - 0.50
W 3.00 4.50

XH65MBy - Detail

Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Mechanical properties of grade XH65MBy

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
712 (≥) 267 (≥) 42 13 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 444

Physical properties of grade XH65MBy

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
521 (≥) 219 (≥) 42 21 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 242
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
932 638 373

Equivalent Grade

Equivalent Products

We can customize the production of XH65MBy grade, contact us for the best solution.