Z4CND22-16-03Az Stainless Steels to NF A 35-574

Z4CND22-16-03Az - Specification & Application

  • NF A 35-574 - Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod

Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod

Chemical composition(wt.%) of Z4CND22-16-03Az grade: to NF A 35-574

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.040
Si - 0.75
Mn - 4.00
P - 0.025
S - 0.010
Cr 21.00 23.00
Mo 2.50 3.50
Ni 15.00 17.00
N 0.05 0.30
Cu - 1.00

Z4CND22-16-03Az - Detail

Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod

Mechanical properties of grade Z4CND22-16-03Az NF A 35-574

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
956 (≥) 926 (≥) 22 31 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 212

Physical properties of grade Z4CND22-16-03Az NF A 35-574

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
866 (≥) 564 (≥) 22 42 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 121
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
463 275 721

Equivalent Products

We can customize the production of Z4CND22-16-03Az grade, contact us for the best solution.