Z5CND27-05Az Stainless Steels to NF A 35-574

Z5CND27-05Az - Specification & Application

  • NF A 35-574 - Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod

Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod

Chemical composition(wt.%) of Z5CND27-05Az grade: to NF A 35-574

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.050
Si - 0.75
Mn - 2.00
P - 0.035
S - 0.025
Cr 26.00 27.00
Mo 1.30 2.00
Ni 4.50 5.00
N 0.05 0.20

Z5CND27-05Az - Detail

Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod

Mechanical properties of grade Z5CND27-05Az NF A 35-574

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
786 (≥) 856 (≥) 43 22 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 344

Physical properties of grade Z5CND27-05Az NF A 35-574

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
171 (≥) 287 (≥) 34 12 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 422
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
322 168 811

Equivalent Grade

Equivalent Products

We can customize the production of Z5CND27-05Az grade, contact us for the best solution.