07X9ЮЦΦ Stainless Steels

07X9ЮЦΦ - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 07X9ЮЦΦ grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.07
Si - 0.80
Mn - 0.80
P - 0.035
S - 0.025
Cr 8.50 10.50
Ni - 0.60
Mo - 0.30

07X9ЮЦΦ - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 07X9ЮЦΦ

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
928 (≥) 878 (≥) 23 23 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 414

Physical properties of grade 07X9ЮЦΦ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
568 (≥) 154 (≥) 34 33 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 111
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
384 878 876

Equivalent Grade

Equivalent Products