1Cr15 Stainless Steels to GB/T 12770 (2002)

1Cr15 - Specification & Application

  • GB/T 12770 (2002) - Welded stainless steel tubes for machine structures
  • GB/T 3280 (2007) - Cold rolled stainless steel sheets and plates
  • GB/T 4237 (1992) - Hot rolled stainless steel sheets and plates
  • GB/T 4239 (1991) - Cold rolled stainless steel and heat resisting steel strips

Welded stainless steel tubes for machine structures

Chemical composition(wt.%) of 1Cr15 grade: to GB/T 12770 (2002)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Si - 1.00
Mn - 1.00
P - 0.035
S - 0.030
Ni - 0.60
Cr 14.00 16.00

1Cr15 - Detail

1Cr15

Mechanical properties of grade 1Cr15 GB/T 12770 (2002)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
177 (≥) 913 (≥) 32 24 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 431

Physical properties of grade 1Cr15 GB/T 12770 (2002)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
532 (≥) 711 (≥) 41 24 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 232
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
925 328 325

Equivalent Grade

Equivalent Products

We can customize the production of 1Cr15 grade, contact us for the best solution.