20CrMnVTiB4-10 Stainless Steels to NF EN 10269

20CrMnVTiB4-10 - Specification & Application

  • NF EN 10269 - Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties

Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties

Chemical composition(wt.%) of 20CrMnVTiB4-10 grade: to NF EN 10269

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.17 0.23
Si - 0.40
Mn 0.35 0.75
P - 0.020
S - 0.020
Cr 0.90 1.20
Ni - 0.20
Mo 0.90 1.10
Ti 0.07 1.50
V 0.60 0.80
Al 0.015 0.080
As - 0.20
B 0.001 0.010
Cu - 0.20
Sn - 0.20

20CrMnVTiB4-10 - Detail

Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties

Mechanical properties of grade 20CrMnVTiB4-10 NF EN 10269

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
412 (≥) 381 (≥) 13 31 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade 20CrMnVTiB4-10 NF EN 10269

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
219 (≥) 752 (≥) 32 21 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 323
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
851 649 644

Equivalent Products

We can customize the production of 20CrMnVTiB4-10 grade, contact us for the best solution.